The surface tension and density of liquid Ag and Ag–Cu alloys were measured with the sessile drop method. The sessile drop tests were carried out at temperatures from 1098K to 1573 K, on cooling (temperature decreasing stepwise) under a protective atmosphere of high purity Ar (6N). The density of liquid Ag and Ag–Cu alloys decreases linearly with increasing temperature, and an increase in concentration of copper results in a lower density. The surface tension dependence on temperature can be described by linear equations, and the surface tension increases with increasing Cu content. The results of the measurements show good agreement with existing literature data and with thermodynamic calculations made using the Butler equation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.