The studies described make it possible to judge the strain – stress state of ceramic articles at different stages of firing and to establish their effect on the thermomechanical properties of the material. The studies showed that the introduction of pyrite cinders into ceramic paste lowers the elastic modulus by 25 – 30% during the initial period (to 400°C) and 4 – 10% in the temperature interval 500 – 1000°C. These data show that pyrite cinders can be used to intensify firing.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.