Abstract

Epoxy shape memory polymers (SMPs) were preparation and their mechanical properties are focused on. Full shape recovery is observed at 150 °C for each polymer, and the SMP with lower hardener content shows a quicker shape recovery speed. In addition to a good thermal stability, glass transition temperature of the polymers increases with increasing hardener content. Of particular attention of DMA test is that the epoxy SMPs show a high storage modulus not only in glass state but also in rubber state. The tension test indicates that both stress at break and corresponding elastic modulus vary with a peak value for the polymers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.