Abstract
The thermomechanical properties of polyurethane-shape memory polymer foam were investigated by the compressive tests. The results are summarized as follows. (1) The material contracts uniformly in the axial direction with the ratio of lateral strain to axial strain 0.4 in the early stage, but about 0.15 thereafter. (2) The deformation resistance is large at low temperature and at high strain rate. (3) In the case of thermomechanical loading, strain is recovered at temperatures in the vicinity of Tg. The rate of strain recovery is 99%. The rate of strain fixity is 100%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.