Abstract

The temperature and strain distributions of the mockup composed of Cu-alloy with distinct structural material (SS316L and China Low Activation martensitic steel (CLAM)) were calculated and analyzed, based on a high heat flux (HHF) test recently reported with heat flux of 3.2MW/m2. The calculated temperature and strain results in the first wall (FW), in which SS316L is as the structural material, showed good agreement with HHF test. By substituting CLAM steel for SS316L the contrast analysis indicates that the thermo-mechanical property for CLAM steel is better than that of SS316 at the same condition. Furthermore, the temperature and strain distributions of the FW were calculated under the condition of normal ITER operation: the surface heat flux is about 0.5MW/m2 and volumetric heating due to neutron radiation is on the order of 15~20 MW/m2.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.