The TL response of KBr:Eu (0.1% Eu) and KBr:Eu,Mg (0.1% Eu, 0.01 and 0.001% Mg) to 254 nm UV light has been studied. Crystals were subjected to different thermal treatments. The Mg concentration and the thermal treatment that produced the best glow curve reproducibility and sensitivity increase were identified. The sensitivity to UV radiation increased by about three times after the optimum thermal treatment. The addition of Mg (0.001%) was responsible for improvements in the reproducibility of the glow curve characteristics for different samples. The glow curves showed two high-temperature peaks above , similar to those observed after exposure to rays, and the TL response was linear for fluences between 15 and .

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.