P-type(Bi0.26Sb0.74)2Te3+3%Te ingots were prepared by cooling at various cooling rates after vacuum melting .In this paper, the chemical composition, structure and thermoelectric properties of the crystals were evaluated by XRD, SEM, EDAX and thermoelectric measurements including Seebeck coefficient, electrical conductivity and thermal conductivity. With increase of cooling rates, Te-rich phase presents in the crystals, the electrical conductivity increases and the Seebeck coefficient decreases. While thermal conductivities of all ingots are all lower than 1.3W/mK. The maximum ZT (T=298K) was 1.12, which was obtained in the p-type(Bi0.26Sb0.74)2Te3+3%Te ingot prepared at a cooling rate of 4K/min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.