Abstract

In this work, CuyBixSb2−x−yTe3 alloys containing a small amount (0.1 vol%) of SiC nano-particles were prepared by spark plasma sintering using mechanical alloying derived powders. It is found that both the electrical resistivity and Seebeck coefficient of (Bi,Sb)2Te3 alloy are significantly decreased by doping a trace Cu and increasing Sb-to-Bi ratio, but the thermal conductivity of (Bi,Sb)2Te3 alloy is also obviously increased by doping a trace Cu, especially at low temperature. A peak ZT value about 1.23 is obtained at 423 K for Bi0.3Sb1.7Te3, in which all ZT values at the whole measuring temperature range are above 1.0. Such ZT characteristics are more attractive for commercial applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.