Abstract

This report describes measurements of thermoelectric power of bismuth vanadium oxide, Bi 4V 2O 11, three samples of Cu 2+ doped bismuth vanadium oxide, Bi 2V 0.95Cu 0.05O 5.425, Bi 2V 0.925Cu 0.075O 5.3875 and Bi 2V 0.9Cu 0.1O 5.35. For these oxides reversible oxygen electrodes were employed which enabled very accurate measurements to be made. Conductivity measurements were also carried out as a comparison to the thermoelectric power results. In addition, EXAFS and high temperature, powder XRD experiments were performed on the samples to investigate any structural phase changes in combination with the electrical studies.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.