Abstract

We measured thermoelectric power (TEP) in the temperature range from 5 to 300 K for heat-treated carbon fibers prepared by chemical vapor deposition of cyanoacetylene on pitch-based carbon fibers. The thermoelectric power of the fiber heat-treated at 2,000°C is positive and exhibits almost monotonic temperature dependence above about 20 K. Thermoelectric power decreases with increasing heat-treatment temperature (HTT), which indicates the formation of graphite structure. TEP for fibers heat-treated over 3000°C have negative dips around 25 K that are ascribed to the phonon-drag effect. TEP for the fiber with 3300°C HTT shows an anomaly near 15 K in addition to the negative dip, suggesting the highly graphitized structure. TEP of the HNO 3-intercalated graphite fiber (HTT; 3300°C) is also measured.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.