Abstract
Thermodynamic properties of aqueous solutions of iota-carrageenan as affected by KCl (0.15-1.2 M) or iota-carrageenan (0.5-6 mg/mL) content were studied by high-sensitivity differential scanning calorimetry. The polysaccharide was found to undergo two consecutive cooperative conformational transitions, which can be represented by the scheme: [H2]2<-->2H2<-->4C where C is the random coil, H2 is the double helix, and [H2]2 is the double helix dimer. The first transition follows by the "all or none" mechanism. The profile of the second transition resembles that of a second-order phase transition. The parameter sigma (of order 1), estimated for this latter transition, suggests that the stacking effect in helices of iota-carrageenan is rather small. The cooperativity of the transition is mainly defined by the loop factor. Free energies of both transitions at 273 K were calculated as a function of salt concentration. These experimental data were found to agree with Manning's theory.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.