Abstract

Copper–β″-alumina was prepared by ion exchange reactions starting with a sodium–β″-alumina. Exchange from sodium ion to copper ion was done by immersing the sample in liquid cuprous chloride. Exchange of Na + ion in β″-alumina to Cu + ion was not complete as Na + ion remained within the β″-alumina. Copper activity in solid copper–nickel alloys was measured by electromotive force (EMF) technique incorporating the partially exchanged (Cu +–Na +)–β″-alumina as a solid electrolyte for temperatures between 870 and 1300 K. The activities of copper and nickel in the solid solution at these temperatures exhibited positive deviations from Raoult's law. The activity coefficients of copper and nickel at infinite dilution at 973 K were estimated to be 5.55 and 3.71, respectively. Furthermore, the free energies, enthalpies and entropies of mixing were derived from EMF data.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.