Abstract
Shale can be a potential buffer for high-level radioactive nuclear wastes. To be an effective buffer while subject to waste heat, shale's mechanical response at elevated temperature must be known. Many researchers have experimentally characterized the mechanical behavior of various shales at different length scales in adiabatic conditions. However, its mechanical performance at elevated temperatures at the nano-scale remains unknown. To investigate the temperature dependency of nanomechanical properties of shale, we conducted both experimental and numerical studies. In this study, we measured mechanical and fracture properties of shale, such as hardness, elastic modulus, anisotropy, and fracture toughness from 25 °C up to 300 °C at different bedding planes. Statistical analysis of the results suggests that hardness and fracture toughness significantly increased at temperatures from 100 to 300 °C; while, temperature does not have a significant impact on elastic modulus. Data also shows that the bedding plane orientations have a substantial impact on both mechanical and fracture properties of shale at the nano-scale leading to distinct anisotropic behavior at elevated temperature below 100 °C. Additionally, we numerically investigated the mechanical performance of the shale samples at room temperature to gain an insight into its mechanical response through the thickness. Numerical results were validated against the experimental results, confirming the simulation can be used to predict shale deformation at the nano-scale or potentially be used in multi-scale simulations.
Highlights
Shale can be a potential buffer for high-level radioactive nuclear wastes
Islam et al conducted a triaxial test at room temperature and showed that the elastic modulus of Pierre-1 shale varies with respect to the orientation a ngles[5]
The mineralogy of the clay fraction is used in the Rietveld refinement of the bulk sample to quantify the abundance of the crystalline phases
Summary
Shale can be a potential buffer for high-level radioactive nuclear wastes. To be an effective buffer while subject to waste heat, shale’s mechanical response at elevated temperature must be known. They tested mechanical properties of Longmaxi formation shale samples before and after exposure to supercritical CO2 and found out that the mechanical properties (i.e., hardness, elastic modulus, and fracture toughness) decreased after the t reatment[13].
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have