Abstract
The performance of a flexible transparent conductive electrode with extremely smooth topography capable of withstanding thermal processing at 300 °C for at least 6 h with little change in sheet resistance and optical clarity is reported. In depth investigation is performed on atomic layer deposition (ALD) deposited ZnO on Ag nanowires (NWs) with regard to thermal and atmospheric corrosion stability. The ZnO coated nanowire networks are embedded within the surface of a polyimide matrix, and the <2 nm roughness freestanding electrode is used to fabricate a white polymer light emitting diode (PLED). PLEDs obtained using the ZnO‐AgNW‐polyimide substrate exhibit comparable performance to indium tin oxide (ITO)/glass based devices, verifying its efficacy for use in optoelectronic devices requiring high processing temperatures.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.