This study presents an approach for synthesizing Eu2+/Eu3+-coactivated Ca2SiO4 nanophosphors, by adjusting the ratio of both activators within a singular host material. Utilizing a hydrothermal method complemented by a postreduction sintering process, we fabricated a series of phosphors characterized by uniform 30-50 nm spherical nanoparticles. These engineered phosphors manifest multichannel luminescence properties and exhibit simultaneous blue and red emission from Eu2+ and Eu3+, respectively. Meticulous control of the 5% H2-95% N2 reduction temperature allowed for precise tuning of the Eu2+ and Eu3+ ions within the host lattice, which enabled the strategic adjustment of their luminescent outputs. Utilizing X-ray photoelectron spectroscopy (XPS), we could discern subtle alterations in the europium oxidation state. By using a transmission electron microscope (TEM) and an X-ray diffractometer (XRD), we found that the subsequent changes by reductive sintering to particle size, morphology, and mixed crystal structures influenced the materials' luminescent characteristics. Our findings herald a significant advancement in solid-state lighting, with the potential for the use of Eu2+/Eu3+-coactivated calcium silicate nanophosphors to develop white light emission technologies endowed with enhanced color rendering and luminous efficacy.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.