Abstract

All-optical switching (AOS) in ferrimagnetic Fe(100-x)Tb(x) alloys is presented. AOS is witnessed below, above, and in samples without a magnetic compensation point. It is found that AOS is associated with laser heating up to the Curie temperature and intimately linked to a low remanent sample magnetization. Above a threshold magnetization of 220 emu/cc helicity dependent AOS is replaced by pure thermal demagnetization.