Abstract

Thermal stress caused by the coefficients of thermal expansion (CTE) mismatch of materials is the main failure mechanism in power electronic packaging. High junction temperature (Tj) would induce larger thermal stress and accelerate failing process. In this paper, two packaging strategies to reduce thermal stress of power module for high-temperature operation were presented based on organic-free sintered Ag bonding and wireless packaging structuring: reduce elastic modulus of sintered Ag layer by changing sintering parameters; and reduce the CTE mismatch by changing the ribbon material. Finite-element analysis (FEA) simulations confirmed that these strategies can effectively reduce the maximum and average thermal stress in power electronics packaging. Furthermore, by combining these two strategies, high-temperature power cycling test indicated that the wireless packaging with Cu30Mo70 ribbon and 5 MPa sintering pressure exhibited excellent durability and reliability in the temperature swing at the junction (ΔTj∆Tj) over 150 K.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.