Abstract

Aluminum foam-Paraffin Composite Phase Change Materials (APCPCMs) were fabricated by aluminum foam and paraffin, and the thermal storage and thermal release properties of the composites have been studied. The results are shown as follows. (1) When the volume ratio between APCPCM and water is 1:4, the time for the temperature changing of APCPCMs with aluminum foam porosity being 54.81%, 60.52%, 64.37% and 69.74%, from 24°C to 66°C, is 190s, 305s, 380s and 395s respectively. The thermal release time of these APCPCMs is 270s, 355s, 540s and 600s after being put into 24°C water, and resulting in a water temperature increase by 8.2°C, 8.7°C, 9.4°C and 10.1°Crespectively. (2) APCPCM with aluminum foam porosity 60.52% is compared with aluminum foam and paraffin, the thermal storage time of these three kinds of materials is 305s, 60s, 870s, and the thermal release time is 355s, 30s, 1470s respectively. (3) The equivalent thermal conductivity coefficient of the APCPCMs with aluminum foam porosity ranging form 69.74% to 54.81% is between 61.16 W•m-1•k-1 to 91.4W•m-1•k-1.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.