Abstract

To enhance the thermal stability of the NiO pinning layers for spin valves, /spl alpha/-Fe/sub 2/O/sub 3/ layers, of which the Neel temperature is 680/spl deg/C for bulk, are deposited on NiO layers. With 15-80 /spl Aring/ thick /spl alpha/-Fe/sub 2/O/sub 3/ layers on NiO layers, an exchange anisotropy field about five times larger than that of NiO/NiFe is obtained after 250/spl deg/C thermal annealing. Spin valve multilayers with NiO//spl alpha/-Fe/sub 2/O/sub 3/ antiferromagnets show about 12% MR ratio. After 150/spl deg/C annealing, the MR ratio changes less than 20% for patterned spin valve multilayers with abutted junctioned hard magnets.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.