Abstract
Bulk metallic glasses (BMGs) with high thermal stability and good corrosion resistance were synthesized in the (Cu0.6Hf0.25Ti0.15)100−x−yNiyNbx system by copper mold casting. The addition of Ni element causes an extension of a supercooled liquid region (ΔTx = Tx – Tg) from 60 K for Cu60Hf25Ti15 to 70 K for (Cu0.6Hf0.25Ti0.15)95Ni5. The simultaneous addition of Ni and Nb to the alloy is effective in improving synergistically the corrosion resistance in 1 N HCl, 3 mass% NaCl, and 1 N H2SO4 + 0.01 N NaCl solutions. The highly protective Hf-, Ti-, and Nb-enriched surface film is formed by the rapid initial preferential dissolution of Cu and Ni, which is responsible for the high corrosion resistance of the alloys in the solutions examined.