Abstract
Ni–10 wt-%Al composite powders, as a self-bonding spray material, were prepared by low energy mechanical milling process and then sprayed by plasma and flame spray techniques. The phase identification, microstructure, hardness and adhesion strength of the coatings were investigated by X-ray diffraction, SEM, ASTM E384-99 and ASTM C633-01 respectively. The size and microstructure of powder particles are two important parameters for thermal spraying. Morphological and microstructural investigation of the Ni–10 wt-%Al powders showed that the powder particles after 23 h of milling time had the optimum properties with respect to their size and microstructure. X-ray diffraction patterns of powder particles included only the elemental Ni and Al peaks without any traces of oxides or intermetallics phases. Powder particles produced by mechanical milling had a fine lamellar structure consisting of pure Al and Ni layers. This structure encourages the Ni/Al exothermic reaction during flight in plasma spraying. The adhesive tests also showed that the plasma and flame failure were cohesive, that is, within the coating itself, because adhesive on steel in both coatings is much higher than cohesive.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.