Abstract

Dynamic mechanical analysis (DMA) measurements of water-saturated earlywood (EW) and latewood (LW) of various wood species in the temperature range from 0 to 100 °C were focused to clarify the differences in thermal softening properties within an annual ring. The following results were obtained. The peak of tanδ caused by micro-Brownian motion of lignin was observed in both EW and LW all species. For softwoods, the peak temperatures of tanδ of EW appeared at higher temperatures than those of LW. For hardwoods, in the other hand, the peak temperatures of tanδ were slightly different between EW and LW in the diffuse-porous wood, whereas the temperatures were almost the same in the ring-porous wood. It was found that the difference in peak temperature of tanδ between EW and LW varied greatly among species. The difference in peak temperature between EW and LW was relatively large for softwoods. In addition, the thermal softening properties both in the radial and tangential directions differed depending on the species, so this suggested that there was anisotropy in the thermal softening properties depending on the species.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.