Abstract
The thermal behavior of tristearin was studied by adiabatic calorimetry and differential scanning calorimetry (DSC). Specific heat capacities of two polymorphic forms were measured in the adiabatic calorimeter, where the β-form was measured from 10 K to 370 K and the α-form was measured from 175 K to 370 K. The start of the measurement of the stable β-form from 10 K allowed the calculation of its entropy, so we report the derived values of absolute entropy for the two forms of tristearin at 298.15 K. The enthalpies of fusion and melting temperatures for each polymorph were calculated from both the adiabatic and the DSC experimental data and are compared to the literature values. The values for the enthalpies of fusion of the stable β-form are in excellent agreement, being (221.6 ± 1) J·g-1 and (219.6 ± 2) J·g-1 according to the adiabatic and DSC measurements, respectively. The data for the α-form are not in so good agreement, which we attribute to the difficulty to crystallize this phase in its pure form....
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.