Abstract
AbstractAn environmentally friendly phenolic resin/Al2O3 hybrid composite was prepared. Al2O3 particles were pretreated with a silcane coupling agent, then the mixture of paraformaldehyde and treated Al2O3 was grinded with ball crusher for several hours, and added during the phenolic resin polymerization process, finally got the hybrid composite. The kinetic parameters of thermal degradation were calculated by the methods of Kissinger, Flynn‐Wall‐Ozawa and Crane. The thermal degradation activation energy of environmentally friendly phenolic resin/Al2O3 hybrid composite is approximate three times of pure phenolic resin. The results show that the heat resistance is obviously improved. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.