AbstractPolyethylene (PE) is one of the most used polymers which can be applied since to flexible packaging to general goods industries, representing 32% of the total market share. Crosslinking PE (XPE) is of considerable practical importance since it increases the upper application temperature limit and improves mechanical performance. The objective of this work was to investigate the thermal degradation kinetics in inert (nitrogen) and oxidative (oxygen) environments of XPEs industrial formulations, with the crosslinking agent content between 0% and 1.5%. PE and XPE specimens were characterized by thermogravimetry (TG) and the computed data modeled using ASTM E698. Increasing the heating rates shifted the degradation rate (dα/dt) and weight loss to higher temperatures, whereas XPEs showed greater thermal stability related to PE. Deconvolution of derivative thermogravimetry (DTG) peaks displayed to be an important tool during kinetics analysis providing understanding and reliable data which affords excellent fits between theoretical and experimental data. In plots acquired using ASTM E698 the degradation activation energy (Ea) increased along with the degradation; morphological and structural changes are suggested in the higher Ea range. Among investigated compounds, 0.5XPE presented the best performance, that is, the greatest thermal stability in both atmospheres.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.