The complex three-dimensional geometry of conventional full crown restorations severely complicates the study of thermal cycling distortion in metal ceramic castings. A simplified experimental geometry was developed to (1) maximize the measuring sensitivity, (2) eliminate the casting variables, (3) allow the direct measurement of casting distortion, and (4) evaluate the thermal cycling distortion of a wide range of metal collar widths. It was found that all of the one-walled castings distorted during the initial thermal cycling (oxidation) of the alloy. There was no significant distortion associated with porcelain application or glazing. The castings with an 0.8 mm metal collar had significantly less distortion than those with 0.1 and 0.4 mm collars at 2 of the 10 sites measured (inferior or facial margins).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.