The thermal conductivity of single-crystal solid solutions (ZrO2)1 – x – y – z(Sc2O3)x(CeO2)y(Y2O3)z (x = 0.08–0.10; y = 0.005–0.01; z = 0–0.005) was measured in the temperature range 50–300 K. Phase composition and defective structure of crystals were studied.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.