Abstract

The thermal conductivity of composites sintered from natural microdiamond (5–7 and 10–14 μm) and nanodiamond powders under pressure of ∼ 6.0 to 6.5 GPa at the temperature ∼ 1000 to 2000 °C for 6–20 s was measured in a steady heat flow in the temperature range of 50–200 °C. It was found that the thermal conductivity of nanodiamond composites produced in these conditions was less than 10 W/(m ⁎К) while that of natural microdiamonds was as high as 500 W/(m ⁎К).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.