Abstract
Upon insertion and extraction of lithium, materials important for electrochemical energy storage can undergo changes in thermal conductivity (Λ) and elastic modulus (M). These changes are attributed to evolution of the intrinsic thermal carrier lifetime and interatomic bonding strength associated with structural transitions of electrode materials with varying degrees of reversibility. Using in situ time-domain thermoreflectance (TDTR) and picosecond acoustics, we systemically study Λ and M of conversion, intercalation and alloying electrode materials during cycling. The intercalation V2O5 and TiO2 exhibit non-monotonic reversible Λ and M switching up to a factor of 1.8 (Λ) and 1.5 (M) as a function of lithium content. The conversion Fe2O3 and NiO undergo irreversible decays in Λ and M upon the first lithiation. The alloying Sb shows the largest and partially reversible order of the magnitude switching in Λ between the delithiated (18 W m−1 K−1) and lithiated states (<1Wm−1K−1). The irreversible Λ is attributed to structural degradation and pulverization resulting from substantial volume changes during cycling. These findings provide new understandings of the thermal and mechanical property evolution of electrode materials during cycling of importance for battery design, and also point to pathways for forming materials with thermally switchable properties.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Current Opinion in Solid State and Materials Science
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.