This study provides analytical results for heat of hydration in the mat foundation with mass concretes to investigate the effect of lift thickness in the mat foundation on the hydration heat and crack characteristics of mat foundation with mass concrete. Mass concretes were mixed with ternary cement with 1% strontium-based latent heat binder at volume fraction and Type IV low heat cement. The mat foundation has the dimension of 15m length, 20m width and 3m depth. Lift thickness of mass concrete for mat foundation was varied from 1.0m to 3.0m. A commercial software MIDAS/Gen was used to analyze the hydration heat of mass concrete foundation. The maximum adiabatic temperature rise (K), and the coefficient of temperature rise (α) for thermal analysis were drawn from adiabatic temperature rise test. Based on the results of the finite element analysis for mat foundation with different lift thickness, the highest internal temperature and thermal stress increased with increasing with lift thickness of foundation. However, for foundation constructed with premixed strontium based latent heat binder (PSLB) concrete, this phenomenon was less remarkable compared to mass concrete foundation made with low heat cement.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.