Abstract

The extent of pyrolysis in partially burnt spruce bark was monitored using a hollocellulose-specific fluorochrome. Fluorescence and hollocellulose content decreased as exposure temperature increased. No fluorescence was observed in material exposed to temperatures above 400 °C. The depth of the pyrolysis front into the bark layer of trees burnt in wildfires helps to determine the fire severity.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.