Abstract

Two samples, a Platreef flotation concentrate and coarse ore (<6 mm), were column bioleached at 65°C using a culture dominated by Metallosphaera hakonensis. Based on solution assays, extractions in excess of 90% Cu and Ni were achieved from the flotation concentrate, while from the coarse ore 96% Cu and 67% Ni extractions were achieved. The difference in extraction levels and leaching patterns despite identical conditions used for both samples is discussed, as is the performance of the samples during a follow-up leach step using cyanide to extract the PGMs in a separate column leach experiment. While the recovery of Pd and Au was excellent during these steps, recovery of Pt was limited to 35% after 45 days for the concentrate and 56% after 60 days for the whole ore material, primarily due to the presence of a refractory Pt mineral. Recovery from a concentrate without pre-treatment was substantially lower.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.