Reagent grade of calcium and magnesium hydroxides were used in this study to treat acid mine drainage (AMD) sample. AMD sample was collected from a tin tailing pond that located in Pengkalan Hulu, Perak which as pH around 2.87 ± 0.01. pH values had increased after treated with calcium hydroxide (Ca(OH)2) and magnesium hydroxide (Mg(OH)2), respectively. The maximum pH values obtained was 11.35 ± 0.01 by using 1.0 g of Ca(OH)2 at interval time 5 min. For Mg(OH)2, the highest pH value can be obtained was 7.22 ± 0.01 by using 1.0 g at interval time 30 min. The concentration of heavy metals such as aluminum, copper, iron, manganese, nickel and zinc were reduced after reaction with both materials. For examples aluminum concentration was reduced from 110.33 mg/L to 2.80 mg/L and 0.01 mg/L by using 1.0 g of Ca(OH)2 and Mg(OH)2, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.