In this study, the PbTe samples doped with PbI2 or Na were prepared using powder metallurgical techniques. The preparation procedures were optimized by the experimental results with respect to powder particle size, compaction pressure, and influence of sintering parameters. The power factor profiles of the PbTe samples with different dopant concentration at about 100°C to 250°C were calculated from the measured values of the Seebeck coefficient and the electrical of the samples. The research interpretation to the thermoelectric properties had been transformed by means of the different dopant concentration indeed. The power factor of the N-type samples was better than the P-type samples. For optimization of the power factors presented in the measurements temperature range, the optimized dopant concentration of PbI2 is 0.05 at% and of Na is 0.50 at% respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.