Abstract
Thermodynamic calculations, which are being performed on a daily basis in industrial laboratories such as the General Electric Corporate Research and Development Center, have proven to be of great assistance in the development of new alloys and the selection of processing conditions for existing or new alloys. This article presents an evaluation of the state-of-the-art ofthat capability for nickel-base superalloys.