Abstract
The surface composition of a series of nickel–chromia catalysts has been examined by X-ray photoelectron spectroscopy. Correlation of the amount of available surface nickel with the activity of the particular catalyst for hydrogen water deuterium isotope exchange is very good. No significant alterations are observed in the valence band spectra as the surface composition changes.