The sulphidation behaviour of high contraction (HC) and low contraction (LC) chromium plated steel was studied in sulphur with a partial pressure of 1 atm at 1, 3, 5 and 7 h and 0.1 and 0.01 atm at 5 h. The temperature was 600°C throughout the work. It was found that HC and LC chromium plating imparted significant sulphidation resistance to steel. It should be mentioned that by increasing sulphidation time and sulphur partial pressure, the hardness of chromium coating decreased. LC chromium coating had a lower thermal shock resistance than the HC coating. Thus, it was concluded that the HC chromium coating had the better sulphidation resistance.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.