In this research, the preparation of nano thin films of mixed NiO with SnO2-CdO various concentrations (،50،2575%) was accomplished. The thin films were prepared by chemical spray pyrolysis method and its" deposited on glass" substrate at a temperature of 200C°. The XRD diffraction displayed the formation of nano composite has a polycrystalline nature. The crystallite size was calculated adopting Scherer’s formula. The optical properties explored decreased transmission for the higher concentration of SnO2-CdO thin films. The energy bandgap values were found with increased concentration of SnO2-CdO. The AFM analysis shows that the roughness increased with increasing mixing of (2.7nm) to (6.23nm) and average grain size of (13.6nm) to (28.6nm). The SEM shows a fine structure of nanoparticles distributed on the surface average size of nanoparticles (46.5nm).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.