Abstract

Semisinusoidal loads with constant amplitude or increasing amplitude were applied on steel specimens separately in earth magnetic field. The testing results indicated that t he variation degree of the magnetic signals was mostly determined by the amplitude of the applied loads. With the load amplitude increasing to plastic loading stage, zero-crossing of the Hp(y) distribution curve occurred and stayed at certain position where the curve has large gradient. The zero-crossing position was exactly the necking point and unchangeable after unloading, which suggested that the plastic failures and microdefect s can be identified through testing the Hp(y) signals.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.