Abstract
The second virial coefficients A2 of ring polystyrenes with high purity in cyclohexane were measured by light scattering in the temperature range 27.0–34.5°C. The purity of four samples with Mw of 16k, 42k, 110k and 570k was determined to be all over 96% by HPLC. It has been found that A2s of all the samples are definitely positive at the theta temperature of linear polystyrene, 34.5°C, and the measured values for four samples converged to zero at 27.7°C with decreasing temperature. This value is below the previously reported one, but it is quite consistent with the predicted value based on the topological repulsive interaction among the ring polymer molecules.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.