Abstract
In this work a heat treatment procedure was performed on laser clad Ti–6Al–4V, which resulted in a reduction of tensile residual stresses in the clad samples as well and a decrease in the hardness of the clad layer with an increasing heat treatment time. The reduction in the residual stress was attributed to inter-phase stress relaxation brought about by the growth of the β phase. The reduction in hardness was attributed to an increase in the volume fraction of the soft β phase. Both the reduction in residual stress and hardness due to this heat treatment makes it an attractive method to heat treat both laser clad and additively manufactured Ti–6Al–4V components for improved mechanical properties.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.