Abstract

Ru–La catalysts with different La/Ru molar ratios were prepared by co-precipitation. Characterizations revealed that the promoter La existed as La(OH)3 on the Ru surface. The La(OH)3 itself could not enhance the selectivity to cyclohexene of Ru catalyst. However, the La(OH)3 could react with ZnSO4 in slurry to form an insoluble (Zn(OH)2)3(ZnSO4)(H2O)3 salt. The chemisorbed (Zn(OH)2)3(ZnSO4)(H2O)3 salt on Ru surface played a key role in improving the selectivity to cyclohexene of Ru catalyst. Ru–La catalyst with the optimum La/Ru molar ratio of 0.14 gave a maximum cyclohexene yield of 59.5%. Besides, Ru–La(0.14) catalyst had a good reusability and an excellent stability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.