Abstract

This paper focuses on the synthesis of rhombohedral B4C (r-B4C) coatings by CO2 laser-assisted chemical vapour deposition (LCVD), using a dynamic reactive atmosphere of BCl3, H2 and CH4 or C2H4. The influence of the carbon precursor on the deposition kinetics is discussed. The use of ethylene as carbon precursor presents several advantages over the use of methane, which is the conventional carbon precursor in CVD processes. These advantages are mainly related to its high absorption coefficient at the laser wavelength and a higher sticking coefficient, which enables to attain higher deposition rates and film thickness control at lower carbon precursor concentration. Films with carbon content from 15 to 22 at.% were grown at a deposition rate as high as 0.12 ∝m.s -1 .

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.