Abstract
High pressure cooling is a new cooling technology, which provides a certain technical support for cutting superalloy. In this paper, the theoretical model of the acting area and force of the coolant under different pressures were established. A theoretical model of the tool-chip contact length in cutting superalloy under high pressure cooling was established by the theory of material mechanics. Through theoretical research and simulation analysis, it is concluded that high pressure coolant can reduce the tool-chip contact length, and with the increase of coolant pressure, the contact length further decreases.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.