Abstract

This study aimed at determining the total yield, screened yield, rejected yield, Kappa number and viscosity of organosolv Acacia hybrid pulp. Acacia hybrid wood chips of uniform size were used to undergo pulping in a digester with five different ethanol concentrations, 50, 60, 70, 80 and 90 % (v/v) with 1 M of sodium hydroxide as catalyst and water. All chips were digested at 185 °C, duration of 3 h cooking time and pressure 1.1–1.2 MPa. It was observed that increasing of ethanol concentration has led to increment in pulp yield and degree of delignification.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.