Abstract
The superplastic deformation uniformity of laser welded joint of TC4 titanium alloy is improved by hydrogen treatment. The non-uniform deformation coefficient K was introduced to quantification ally characterize the non-uniform deformation. The results show when the content of hydrogen exceeds 0.29%, the super plasticity of the titanium alloy welded plate decreases with the increase of the hydrogen content. The decrease of the shrinkage of the base material is larger than that of the weld section with the increase of hydrogen content. The K can be used to describe the non-uniform deformation of the weld and the base material during the superplastic deformation of laser welded joint of the TC4. The K value increases with increaseing hydrogen content, increaseing deformation temperature and decreaseing strain rate. The K value reaches the maximum of 0.84 with hydrogen content of 1.299%, deformation temperature of 920 °C, strain rate of 10-4S-1.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.