Abstract

In this paper, the relationship between the tensile ductility loss and the conditions including the exposure process and microstructures for the hot exposed TiAl alloys was researched. The critical temperature corresponding to the ambient tensile ductility loss to 0.8% was sensitive to the microstructure. It was 800°C/100h exposure for the near fully lamella microstructure. Due to the oriented lamella, the near fully lamella microstructure was benefit for forming the oxide layer rich in Al to present further oxidation of the matrix.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.