Three different kinds of MnOx desulfurization sorbent were prepared by different calcination temperature and reduction method. The properties of H2S removal and COS formation over the prepared MnOx were measured in the fixed bed at 550°C, and the MnOx phases before and after desulfurization were characterized by XRD and XPS. The results show that the sequence of the amount of COS formation over three MnOx samples is Mn3O4>Mn2O3>MnO, and the sequence of H2S penetration time is Mn3O42O32 are good for COS formation. With the single sulfur and MnS2 accumulated in MnOx desulfurization sorbent, the more and more the amount of COS formed during desulfurization.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.