Abstract

LaF3 powder is prepared by means of three methods . The traditional precipitation of LaC13 with HF action, sol-gel of La (CH3COO) 3 with NH4F action then gel is handled by infrared furnace and microwave method of La (CO3)3 as La source with NH4F action to become LaF3 Ultra-fine powder under the action of microwave. Through the SEM photographs, it can be revealed that the powder particles are different. Precipitation particles diameter is 10 μm; sol-gel method of particle is 1 um and there are a lot of needle-like particles; microwave particles is 100nm.