Abstract

This study is the continuation of the first part (Horváth et al. 2023), in which density, bending strength and modulus of elasticity of 100 oak lamellae generated as small-sized production waste were investigated. In this part of the study series, the classification of our sample set is carried out according to the EN 338. A visual pre-grading is presented, to remove the worst specimens and achieve a better final result and a standardized visual grading is also shown. Our results are compared with literature values of clear specimens as well. Amount of 80% of the specimens were found to be suitable for further structural use. The total sample set is classified in strength class D35 (average density 712.6±72.5 kg/m3; average MoRadj 65.4±16.2 MPa; average MoEadj 13.4±3.1 GPa), while the visually pre-graded part with better average test results is classified in strength class D45. Industrial wood residues contain a sufficiently high proportion of elements for further processing, so that after sorting it can be used as raw material for glued-laminated load-bearing timber.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call